Solid Solution Strengthening for Mg-3.0 Mass Pct (2.71 At. Pct)Al and Mg-0.06 Mass Pct (0.036 At. Pct)Ca AlloysChino · Metallurgical and Materials Transactions A2010PDF741 KB
Examination and Analysis of 2 Pct Mg-55 Pct Al-1.6 Pct Si-Zn Coating on SteelChen · Metallurgical and Materials Transactions A2020PDF3.6 MB
Evolution of Microstructure and Tensile Strength of Rapidly Solidified Al-4.7 Pct Zn-2.5 Pct Mg-0.25 Pct Zr-X Wt Pct Mn AlloysChang · Metallurgical and Materials Transactions A1998PDF716 KB
Mechanical properties of a 29 Pct Cr-4 Pct Mo-2 Pct Ni ferritic stainless steelNichol · Metallurgical Transactions A1977PDF2.7 MB
Dynamic Recrystallization During Creep in a 45 Pct Ni-35 Pct Fe-20 Pct Cr Alloy SystemKoul · Metallurgical Transactions B1985PDF1.6 MB
High strain rate superplasticity of a 25 Wt Pct Cr-7 Wt Pct Ni-3 Wt Pct Mo-0.14 Wt Pct N duplex stainless steelMaehara · Metallurgical and Materials Transactions B1991PDF3.6 MB