Adâncimea de Așchiere: Experimente și Date by Tudor Ratiu is a document available to read on EtoBox.
The document describes the results of 4 cutting experiments. Experiment 1 had a diameter of 58mm, 500 rpm speed, 0.1mm feed, 1mm depth, and measured cutting, resisting, and advancing forces along with a 381 degree temperature. Experiment 2 increased the feed to 0.2mm and measured increased forces and a 376 degree temperature. Experiment 3 increased the speed to 800 rpm and measured slightly lower forces and a 397 degree temperature. Experiment 4 returned to a 0.1mm feed but decreased the depth to 0.5mm, and