Nickel Sulphide Inclusions in Glass by marie is a document available to read on EtoBox.

This technical note discusses nickel sulphide (NiS) inclusions in toughened glass, which can lead to breakages due to a phase change that occurs at high temperatures. The document outlines the history of NiS research, the mechanisms of fracture, and the development of heat soaking processes to mitigate risks associated with NiS inclusions. It also details the formation of NiS inclusions, their critical sizes for causing breakage, and the timescale for breakages in service.