8D Corrective Action Report Summary by Wilmer Enario is a document available to read on EtoBox.

1. Supplier A issued a corrective action report regarding defects found in case top parts supplied to Customer A. 9 parts out of 500 were rejected due to dents near screw holes, a rejection rate of 1.8%. 2. An investigation determined the dents were likely caused by foreign material stuck in the mold during the pressing process that was not fully removed during cleaning. 3. Containment actions included re-inspecting Customer A