Can I read Fretting wear in titanium, Monel-400, and cobalt : 25-percent molybdenum using scanning electron microscopy on EtoBox?

Fretting wear in titanium, Monel-400, and cobalt : 25-percent molybdenum using scanning electron microscopy by Bill, Robert C. is a nonfiction available to read on EtoBox.

What is Fretting wear in titanium, Monel-400, and cobalt : 25-percent molybdenum using scanning electron microscopy about?

Damage scar volume measurements taken from like metal fretting pairs combined with scanning electron microscopy observations showed that three sequentially operating mechanisms result in the fretting of titanium, Monel-400, and cobalt - 25-percent molybdenum. Initially, adhesion and plastic deformation of the surface played an important role. This was followed after a few hundred cycles by a fatigue mechanism which produced spall-like pits in the damage scar. Finally, a combination of oxidation and abrasion by debris particles became most significant. Damage scar measurements made on several elemental metals after 600,000 fretting cycles suggested that the ratio of oxide hardness to metal hardness was a measure of the susceptibility of a metal to progressive damage by fretting

Who reads Fretting wear in titanium, Monel-400, and cobalt : 25-percent molybdenum using scanning electron microscopy?

It is typically read by self-directed learners exploring a subject in depth.

Common subject areas: history, science, philosophy, social sciences.

Author
Bill, Robert C.
Publisher
National Aeronautics and Space Administration : [For sale by the Clearinghouse for Federal Scientific and Technical Information, Springfield, Virginia 22151], 1972.
Published
1972
Language
EN
Category
nonfiction

More by Bill, Robert C.

Browse all works by Bill, Robert C.

Similar books