Five samples of material were tested before heating to determine their tensile strength. The samples had thicknesses between 1.05-1.12mm and widths of 6mm. When pulled at 200mm/min, they withstood forces of 0.12-0.14kN and had tensile strengths ranging from 19.7-21.44MPa, with an average of 20.42MPa. All samples showed 0% elongation.