Skip to content

Opening book details…

Can I read Tear Test Results Summary on EtoBox?

Tear Test Results Summary by Keishun Andoy is a document available to read on EtoBox.

What is Tear Test Results Summary about?

The document presents the results of a tear test, detailing the thickness, width, maximum tear strength, and strain for various samples. The total average maximum tear strength is 49.24 N/mm with a standard deviation of 9.25, while the total average strain is 181.67%. The results are certified by the testing personnel, confirming the accuracy of the specifications obtained.

Author
Keishun Andoy
Language
EN

More by Keishun Andoy